Surface instability under ambient conditions in layered sodium transition metal oxides, such as P2 type Na2/3[Fe1/2Mn1/2]O2 (NFM), leads to initial capacity loss, poor cyclability, and gelation of the polyvinylidene fluoride slurry through defluorination. Although NFM is a high-performance cathode material,